Skip to main content

Info Supplier Plate/Pipe



Tanya - Rizal
Dear milister,

Mohon info supplier utk pembelian material plate atau pipe yg bisa beli cara potongan ber-mill certificate. Utk carbon steel (A283-C/A516 70/A106-B maupun stainless steel (A240 304 atau 316L /A312 TP304 atau TP316L

Terima kasih sebelumnya.


Tanggapan 1 - Eko Susilo

Bisa menghubungi Acerinox Indonesia Mas di ignacio.gutierrez@acerinox.com, atau bisa juga ke Sutindo, Pratiwi Prima Baja.


Tanggapan 2 -

Dear Pak Rizal,

Coba silahkan cek PT. Jindal Stainless Indonesia, lokasi plant nya di gresik.

Tanggapan 3 - 


Pak Rizal,
Bisa ke Pak Adi Wijaya di 021-62320364. Hanya, kalau mill certificate, musti beli dulu baru diberikan.
Saya juga lagi cari SS 316 Sheet thickness 0,5. Dipasaran adanya yang SS316 L (Low Carbon) 0,5.

Comments

  1. maaf jika berkenan saya ingin bertanya
    saya sedang mengerjakan skripsi tentang pengembangan lapangan panasbumi

    yang ingin saya tanyakan, saya ingin memakai pipa tipe SAW API 5L grade B, untuk ukuran 10" - 30" berapakah kisaran harganya per ton (include shipping)?

    saya sudah cari di internet tapi belum mendapatkan hasil yang memuaskan
    kalau ada yang berkenan memberi tahu bisa email saya di pramadhio.ari@gmail.com

    terima kasih

    ReplyDelete

Post a Comment

Popular posts from this blog

DOWNLOAD BUKU: THE TRUTH IS OUT THERE KARYA CAHYO HARDO

  Buku ini adalah kumpulan kisah pengalaman seorang pekerja lapangan di bidang Migas Ditujukan untuk kawan-kawan para pekerja lapangan dan para sarjana teknik yang baru bertugas sebagai Insinyur Proses di lapangan. Pengantar Penulis Saya masih teringat ketika lulus dari jurusan Teknik Kimia dan langsung berhadapan dengan dunia nyata (pabrik minyak dan gas) dan tergagap-gagap dalam menghadapi problem di lapangan yang menuntut persyaratan dari seorang insinyur proses dalam memahami suatu permasalahan dengan cepat, dan terkadang butuh kecerdikan – yang sanggup menjembatani antara teori pendidikan tinggi dan dunia nyata (=dunia kerja). Semakin lama bekerja di front line operation – dalam hal troubleshooting – semakin memperkaya kita dalam memahami permasalahan-permasalahan proses berikutnya. Menurut hemat saya, masalah-masalah troubleshooting proses di lapangan seringkali adalah masalah yang sederhana, namun terkadang menjadi ruwet karena tidak tahu harus dari mana memulainya. Hal tersebut

[Lowongan Kerja] QA System Coordinator, Pipe Yard Coordinator, Customer Assistant Coordinator

With over 30 years' experience, Air Energi are the premier supplier of trusted expertise to the oil and gas industry. Headquartered in Manchester UK, Air Energi has regional hubs in Houston, Doha, Singapore and Brisbane. We have offices in 35 locations worldwide, experience of supply for 50 countries worldwide, and through our company values: Safe, knowledgeable, innovative, passionate, inclusive, and pragmatism, WE DELIVER, each and every time. At the moment we are supporting a multinational OCTG processing operation in seeking of below positions: 1.       QA System Coordinator Coordinates Quality System development in plant, directing the implementation of specifications and quality norms. Administers complaints regarding non-conformities and provides quality process information in support of decision making. Develops the necessary procedures, instructions and specifications to ensure Quality System conformity. Coordinates and organizes the execution of interna

Efek korosi dari pembakaran NH3 + H2S di Furnace

Complete combustion H2S membutuhkan temperatur antara 625 s/d 1650 degC tergantung komposisi acid gas.  Namun, temperatur minimum untuk efektivitas operasi adalah 925 degC.  Dibawah temperatur ini biasanya  stabilitas flame tidak bagus dan sering muncul free O2 di flue gas.  Untuk kasus Pak Novriandi, free O2 di flue gas harusnya gak masalah karena akan langsung terbuang melalui stack (berbeda jika kondisi ini terjadi di unit pengolah acid gas yang akan menyebabkan korosi di waste heat boiler); namun, dengan temperatur furnace yang Pak Novriandi punya sebesar 843 degC, kemungkinan akan menyebabkan flame menjadi tidak stabil. Tanya - Novriandi   Ysh, Bpk & Rekan Migas Indonesia Kami memiliki equipment furnace dengan servicenya adalah pemanas process, Furnace tersebuttipe vertical tube multi coil dengan material tube inlet A335 P9 dan tube oult A312 TP316. dengan fuel sesuai design adalah kombinasi fuel oil dan fuel gas. Pada kasus tertentu di salah satu unit untuk mengolah dan